Polymer Property : Specific Gravity = 2.27 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.27 g/cc
2.27 g/cc
ASTM D792
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet)
Specific Gravity 2.27 g/cc
2.27 g/cc
ASTM D792
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)  (Unverified Data**)
Specific Gravity 2.27 g/cc
2.27 g/cc
ASTM D4745
3M Dyneon™ CC174/N Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of 15% fiberglass & 5% natural molybdenum disulfide blended with PTFE.Information provided by Dyneon, A 3M Company
Specific Gravity 2.27 g/cc
2.27 g/cc
ASTM D792
Greene Tweed Avalon® 16 PTFE, Glass, Molybdenum Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..
Specific Gravity 2.27 g/cc
2.27 g/cc
BCC Products BC 7009-2 Epoxy Casting
BC 7009-2 is an iron filled, low-cost mass casting system. Recommended for use in casting a minimum of two inches and a maximum of six inches in non-conductive molds. Thicknesses to nine inches in m..
Specific Gravity 2.27 g/cc
2.27 g/cc
Aremco Pyro-Paint™ 634-AL High Temperature Refractory Coating
This pure, alumina based compound creates a hard, high temperature resistant coating for refractory fiber boards and shapes, providing exceptional resistance to molten metals and open flames to 3200..