Polymer Property : Specific Gravity = 2.29 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.29 g/cc
2.29 g/cc
P & P Technology MS-N Nickel Graphite Conductive Adhesive
P & P Technology conductive nickel/graphite adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exp..
Specific Gravity 2.29 g/cc
2.29 g/cc
uncured
Atom Adhesives AA-BOND F162 Epoxy Adhesive
AA-BOND F162 is a thixotropic electrical insulating epoxy adhesive system with low vapor pressure and outgassing characteristics. AA-BOND F162 was specifically developed for fiber optic, laser, phot..