Polymer Property : Specific Gravity = 2.32 g/cc
Polymer Property :
Specific Gravity =
2.32 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Specific Gravity
2.28
-
2.32
g/cc
2.28
-
2.32
g/cc
ASTM D792
Adamas Adalon® 808 PTFE, Bronze + PEEK+ Carbon Fiber