Polymer Property : Specific Gravity = 2.63 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.63 g/cc
2.63 g/cc
KaMin KaMin® 100C Kaolin Clay - Calcined
Calcined clay with new and unique processing and packaging, designed for applications requiring low moisture, such as 2 component urethanes. Prevents the need to pre-dry the mineral.Industry: Adhesi..
Specific Gravity 2.63 g/cc
2.63 g/cc
KaMin KaMin® 2000C Kaolin Clay - Calcined
Highest brightness, smallest particle size, calcined kaolin clay, more cost -effective Ti02 extender than KaMin® 70C.Industry: Paint & CoatingsUses: Architectural Coatings, Industrial Coatings, F..
Specific Gravity 2.63 g/cc
2.63 g/cc
KaMin Nylok® 171 Kaolin Clay - Surface Treated
Amino silane treated calcined kaolin that reinforces polyamide resin systems.Industry: Rubber & PlasticUses: Non-Black Rubber, Nylon, Thermoset, ThermoplasticInformation provided by KaMin LLC.
Specific Gravity 2.63 g/cc
2.63 g/cc
KaMin Polyfil® 80 Kaolin Clay - Calcined
Higher brightness, medium particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber GoodsInformation provided by KaMin LLC.
Specific Gravity 2.63 g/cc
2.63 g/cc
KaMin Polyfil® 90 Kaolin Clay - Calcined
Highest brightness, smallest particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, Butyl Rubber, General Plastics, Polyolefins/PVC, Thermoset, Thermo..