Physical Properties Metric English Comments
Specific Gravity 3.37 g/cc
3.37 g/cc
Epoxy Technology EPO-TEK® H37-MPT Epoxy
Material Description: A single component, silver-filled and electrically conductive adhesive designed for semiconductor die attach and bonding SMDs for hybrid microelectronic packaging. It is certi..