Polymer Property : Specific Gravity = 3.75 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 3.75 - 4.25 g/cc
3.75 - 4.25 g/cc
Parker Chomerics CHO-SEAL 1240 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Specific Gravity 3.75 - 4.25 g/cc
3.75 - 4.25 g/cc
Parker Chomerics CHO-SEAL 1278 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Specific Gravity 3.75 g/cc
3.75 g/cc
Ecomass® 1002ZC85 Stainless Steel Filled COPA
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.Stainless Steel Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Pol..