Polymer Property : Specific Gravity = 4.15 g/cc
Polymer Property :
Specific Gravity =
4.15 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Specific Gravity
3.65
-
4.15
g/cc
3.65
-
4.15
g/cc
Parker Chomerics CHO-SEAL E6434 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics