Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 4.20 - 4.30 g/cc | 4.20 - 4.30 g/cc | |
Reade Advanced Materials Ilmenite Powder (FeTiO3) Description: A naturally mined iron titanium oxide mineral. It is generally black as sand, odorless, tasteless, opaque under a microscope, non-flammable and insoluble at 20 deg. C. Physical Properti.. |
|||
Specific Gravity | 4.20 g/cc | 4.20 g/cc | |
Lord Adhesives Thermosetâ„¢ MD-110 Conductive Adhesive LORD Thermosetâ„¢ MD-110 silver-filled conductive adhesive offers excellent electrical conductivity and room temperature stability. It is designed for use with automated dispensing, stamping and.. |
|||
Specific Gravity | 4.20 g/cc | 4.20 g/cc | |
Tra-Con Tra-Bond RO7 Radio Opaque Epoxy Adhesive TRA-BOND RO-7 is a high viscosity epoxy resin system specifically developed for adhesive and coating applications where radio opacity is required. It can be used as an X-ray marker on in-vitro medic.. |
|||
Specific Gravity | 4.20 g/cc | 4.20 g/cc | |
Excalibar NewBar™ API Barite BaSO4 Powder NewBar™ API barite product is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas explorati.. |
|||
Specific Gravity | 4.20 g/cc | 4.20 g/cc | |
CIMBAR BARA 200 Barium Sulfate (BaSO4) BARA 200 is a natural barium sulfate. Cimbar's BARA 200 is designed to meet all the requirements of drilling grade barite. Bara meets or exceeds all API requirements. These properties make BARA 2.. |
|||
Specific Gravity | 4.20 g/cc | 4.20 g/cc | |
CIMBAR BARA 325 Barium Sulfate (BaSO4) BARA 200 is a natural, off-white barium sulfate. Cimbar's BARA 325 is a clean, high purity, high specific gravity, low solubility barium sulfate and it is chemically inert. These properties have m.. |