Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 4.99 g/cc | 4.99 g/cc | ASTM D792 |
PolyOne Gravi-Tech™ GRV-NY-050-CU-NAT Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Specific Gravity | 4.99 g/cc | 4.99 g/cc | ASTM D792 |
PolyOne Gravi-Tech™ GRV-TP-050-CU-NAT Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |