Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 6.88 g/cc | 6.88 g/cc | ASTM D792 |
PolyOne Gravi-Tech™ GRV-PB-069-BMX Natural Polyether Block Amide (PEBA-Ether) Information provided by PolyOne |
|||
Specific Gravity | 6.88 g/cc | 6.88 g/cc | ASTM D792 |
PolyOne Gravi-Tech™ GRV-NP-069-BMX Nylon 12
(discontinued **) |