Physical Properties Metric English Comments
Specific Gravity 7.73 g/cc
7.73 g/cc
Latrobe LSSâ„¢ D5 Tool Steel (ASTM D5)
TLS D5 tool steel is an air hardening, high-carbon, high-chromium, tool steel that is characterized by a cobalt addition which provides unique resistance to galling and pick-up. The cobalt also impa..
Specific Gravity 7.73 g/cc
7.73 g/cc
ATI Allegheny Ludlum 420 Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..