Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.77 g/cc | 7.77 g/cc | |
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
Specific Gravity | 7.77 g/cc | 7.77 g/cc | |
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
Specific Gravity | 7.77 g/cc | 7.77 g/cc | |
Carpenter No. 883® Hot Work Die Steel (Red-Tough) (AISI H13) No. 883 hot work die steel is a 5% chromium hot work tool steel designed particularly for applications requiring extreme toughness combined with good red-hardness. It has given an extra margin of sa.. |