Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.87 g/cc | 7.87 g/cc | |
Latrobe LSSâ„¢ D3 Tool Steel (ASTM D3) TLS D3 tool steel is a high-carbon, high-chromium, oil-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, large, chromium-rich alloy carbides in the mi.. |
|||
Specific Gravity | 7.87 g/cc | 7.87 g/cc | |
Carpenter No. 484® (Carpenter Air-Hard; AISI A2) No. 484 tool steel is an air hardening steel capable of hardening throughout in heavy sections. It has been used for those applications in which the sections are very large and those involving extre.. |