Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.90 g/cc | 7.90 g/cc | ASTM D792 |
Ecomass® 4703ZD90 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polym.. |