Polymer Property : Specific Gravity = 8.16 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 8.16 g/cc
8.16 g/cc
Carpenter Micro-Melt® M-3 Class 2 Alloy (AISI M3)
Micro-Melt® M-3 Class 2 alloy is a powder metal tungsten-molybdenum high-speed steel possessing the superior wear resistance characteristics required for difficult cutting operations. The advantage..