Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 8.91 g/cc | 8.91 g/cc | |
Lucas-Milhaupt Silvaloy® A24 Brazing Alloy Silvaloy A24 does not contain cadmium and is a lower silver modification to the standard Bag-20 at 30 percent. Its slightly higher melt temperature provides improved mechanical strength when exposed.. |