Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 9.06 g/cc | 9.06 g/cc | |
Lucas-Milhaupt Silvaloy® B72 Brazing Alloy Silvaloy B72 is the eutectic composition of the silver-copper system. It is suitable for use in controlled atmosphere brazing without the use of a paste flux. When molten, it is very fluid and may f.. |