Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 2.0 - 4.0 µm | 2.0 - 4.0 µm | |
Zircar Ceramics AB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Filament Diameter | 2.0 - 4.0 µm | 2.0 - 4.0 µm | |
Zircar Ceramics MB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |