Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 14 - 26 µm | 14 - 26 µm | |
AGY VeTron® Glass Fiber Launched 2002, for Vinyl Ester and Polyester resins. Binder is VE1 silane for Vinyl Esters. Acid resistant. Moderate alkali resistance.Information provided by AGY Holding Corp. |