Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 3.0 µm | 3.0 µm | Mean Fiber Diameter |
Zircar Ceramics ALBF-1 Alumina Bulk Fiber Type ALBF-1 Alumina Bulk Fiber is a specially cleaned alumina fiber with relatively short fiber lengths. It is suitable for use in vacuum forming of high density rigid boards & shapes, in the reinfo.. |
|||
Filament Diameter | 3.0 - 5.0 µm | 3.0 - 5.0 µm | |
Zircar Refractory Composites RSBL-SOL6 Silica-Magnesia Blanket ZIRCAR Refractory Composites, Inc. insulating blankets are non woven, inorganic, fiber-based products that contain no asbestos. They are engineered for use as thermal barrier materials in high tempe.. |
|||
Filament Diameter | 3.0 - 5.0 µm | 3.0 - 5.0 µm | |
Zircar Refractory Composites RSBL-SOL8 Silica-Magnesia Blanket ZIRCAR Refractory Composites, Inc. insulating blankets are non woven, inorganic, fiber-based products that contain no asbestos. They are engineered for use as thermal barrier materials in high tempe.. |
|||
Filament Diameter | 3.0 - 5.0 µm | 3.0 - 5.0 µm | |
Zircar Refractory Composites RSMAT-3000 ALUMINA MAT ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot a.. |
|||
Filament Diameter | 3.0 - 4.0 µm | 3.0 - 4.0 µm | |
Zircar Refractory Composites RS-SI SILICA MOLDABLE ZIRCAR Silica Moldable Type RS-SI Moldable is a wet blanket that is a combination of high purity amorphous silica fibers and inorganic silica binder. The fibers are 6-9 um in diameter and are consid.. |
|||
Filament Diameter | 3.0 - 3.5 µm | 3.0 - 3.5 µm | Median Fiber Diameter |
Zircar Ceramics Alumina Mat A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between.. |