Polymer Property : Filament Diameter = 508 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Filament Diameter 508 µm
508 µm
Mid-Mountain Materials SILTEX® XS-150 Silica Yarn
SILTEX® SILICA YARN XS-150 is comprised of continuous filament, amorphous silica fibers and offers superior protection in electrical applications, as well as excellent resistance to thermal shock..