Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 7.2 µm | 7.2 µm | |
Zoltek Panex 35® 50k Continuous Tow Commercial Carbon Fiber for Industrial Applications Commercial Carbon Fiber for Industrial Applications |
|||
Filament Diameter | 7.2 µm | 7.2 µm | |
Zoltek Panex 35® Milled Carbon Fibers Milled Carbon FibersApplications include: Buoyancy, RFI/EMI Shielding, Static Dissipation, Surface Reinforcement, Low Cost Polyurethane Friction Compounds |
|||
Filament Diameter | 7.2 µm | 7.2 µm | |
Zoltek Panex 35® Tow Weave Carbon Fiber Fabrics Tow Weave Carbon Fiber Fabrics |