Polymer Property : Filament Diameter = 8.0 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Filament Diameter 8.0 µm
8.0 µm
SGL Carbon Group SIGRAFIL C® C10 M250 UNS Milled Carbon Fiber, Unsized Carbon Fiber
Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG..
Filament Diameter 8.0 µm
8.0 µm
Zircar Ceramics ASB-2300 Alumina-Silica Blanket
Useful to temperatures of 1260°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics.