Polymer Property : Saybolt Viscosity at 100°F = 315 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 315 SUS
315 SUS
Lubriplate 3000-W Moly-Lithium Type Multi-Purpose Grease
Tacky, moly-lithium, extreme pressure greases that provide a durable, tenacious, adhesive film to protect against water, rust, and corrosive contaminants. 3000-W is for cold ambient temperatures.App..
Saybolt Viscosity at 100°F 315 SUS
315 SUS
Lubriplate 68-P Semi-Synthetic Refrigeration Compressor Oil
These highly refined lubricants are formulated for use in refrigeration compressor systems utilizing ammonia, CFC (chlorofluorocarbon) and HCFO (hydrochlorofluorocarbon) refrigerants such as R-717, ..