Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 364 SUS
364 SUS
Lubriplate 68 SYN High Temp 100% Ester-Based Multi-Purpose Synthetic Fluid
These 100% ester-based synthetic lubricants are recommended for applications that are exposed to high operating temperatures and must maintain a clean lubricated surface. Available in ISO viscosity ..