Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 4900 SUS | 4900 SUS | |
Lubriplate SFGO Ultra-1000 PAO-Based Synthetic Food Machinery Grade Fluid Polyalphaolefin (PAO)-based high-performance fluids formulated with 100% PAO synthetic base fluids for a variety of demanding applications. They are outstanding lubricants for use under severe condi.. |