Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 560 SUS | 560 SUS | |
Lubriplate PM 500 White Oil USP Mineral -Based Food Machinery Grade This oil contains emulsifying agents that wet the lubricated surfaces and provide an oily film for the moving parts. Used very successfully on pear machines.Available in Bottles, Jugs, Pails, 1/4 Dr.. |