Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 128 cSt | 128 cSt | |
Lubriplate HP-2 Poly Polyurea-Thickened Type Grease For Special Applications / Conditions Polyurea-thickened type grease formulated with the highest quality paraffinic base oils available. Excellent for high speed electric motor bearings and other industrial applications. Applications: E.. |