Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 15 cSt
15 cSt
ASTM D445
Solvay Specialty Polymers FOMBLIN® Y04 PFPE Lubricant
FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati..