Polymer Property : Kinematic Viscosity at 40°C (104°F) = 183 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 183 cSt
183 cSt
Lubriplate 1200-2 Lithium Type Multi-Purpose Grease
This is a heavy-duty general purpose lithium type grease for both industrial and automotive applications. It provides a high film strength, shear stability, and AW & EP additives. Applications: Gene..