Saybolt Viscosity at 210°F 64 SUS
64 SUS
Lubriplate PM 500 White Oil USP Mineral -Based Food Machinery Grade
This oil contains emulsifying agents that wet the lubricated surfaces and provide an oily film for the moving parts. Used very successfully on pear machines.Available in Bottles, Jugs, Pails, 1/4 Dr..