Polymer Property : Kinematic Viscosity at 100°C (212°F) = 16.2 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 13.8 - 16.2 cSt
13.8 - 16.2 cSt
1.23%, ENJ411; BAM 1201
Kraton® G1740 M (SEP) Star Polymer
Description: Kraton G1740 M is a clear, star polymer based on styrene and ethylene/propylene with a polystyrene content of 6%. It is supplied from North America in the physical form identified: Krat..