Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 10.04 cSt | 10.04 cSt | ASTM D 445 |
ConocoPhillips Hydroclear® 10 Ultra-Clean Spindle Oil Description: Conoco Hydroclear Ultra-Clean Spindle fluids comprise blends of special base oils and additives specially formulated for use in applications where a lubricant combining the properties o.. |