Kinematic Viscosity at 40°C (104°F) 13300 cSt
13300 cSt
Base Oil; ASTM D445
Nye Lubricants 875MS (FG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 13300 cSt
13300 cSt
Base Oil; ASTM D445
Nye Lubricants 875MS-UV (FG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 13300 cSt
13300 cSt
Base Oil; ASTM D445
Nye Lubricants 875MS-G0 (FG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 13300 cSt
13300 cSt
Base Oil; ASTM D445
Nye Lubricants 875R (FG) Synthetic Oil
Information provided by Nye Lubricants.