Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
ChevronTexaco Taro® 20 DP SAE 40 Texaco Taro 20 DP delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |
|||
Kinematic Viscosity at 40°C (104°F) | 135 cSt | 135 cSt | |
ChevronTexaco Taro® 30 DP SAE 40 Texaco Taro 30 DP delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |