Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 14.1 cSt | 14.1 cSt | ASTM D445 |
ExxonMobil 446 Mobilmet 440 Series Mobilmet 440 Series fluids are high performance, multi-service, non-corrosive straight cutting fluids. They are designed for moderate to heavy duty cutting operations. They are also suitable for m.. |
|||
Kinematic Viscosity at 40°C (104°F) | 14.1 cSt | 14.1 cSt | ASTM D445 |
ExxonMobil 446 Mobilmet 440 Series Mobilmet 440 Series fluids are high performance, multi-service, non-corrosive straight cutting fluids. They are designed for moderate to heavy duty cutting operations. They are also suitable for m.. |