Kinematic Viscosity at 40°C (104°F) 14.2 cSt

@Temperature 40.0 °C
14.2 cSt

@Temperature 104 °F
ASTM D445
PolyOne Synplast™ DIDA-E Di Isodecyl Adipate
Branched C10 adipate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne
Kinematic Viscosity at 40°C (104°F) 14.2 cSt
14.2 cSt
ASTM D445
ExxonMobil Mobil Aero HFS
Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc..
Kinematic Viscosity at 40°C (104°F) 14.2 cSt
14.2 cSt
ASTM D445
ExxonMobil Mobil Aero HFS
Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc..