Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil; ASTM D445
Nye Lubricants 5301 (SVLG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil; ASTM D445
Nye Lubricants 572H-10 Dispersion
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil; ASTM D445
Nye Lubricants 717E(RL) Rheolube Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8980 (499) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8981 (899-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8981R (899RP-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8981S (899S-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8981SR (899S-1-RP) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8981X (899XP-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
ASTM D445
ExxonMobil Mobil Delvac 50 Synthetic Transmission Fluid
Mobil Delvac Synthetic Transmission Fluid 50 is a fully synthetic, manual transmission lubricant engineered to meet the most demanding extended drain and OEM warranty requirements. It is recommended..
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil
ConocoPhillips Tacna® 2000 NLGI No. 2
Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o..
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
ELM® Bar & Chain Lubricant Biodegradable –Biobased Bar & Chain Lube
Description: ELM Biotechbased™ Bar & Chain Oil is a high quality biodegradable bar and chain saw lubricant formulated with the best optimized biotechnology using USA-grown natural seed oil that sur..
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
ASTM D445
ChevronTexaco Delo® SAE 80W-90 Gear Lubricant ESI®
FeaturesChevron Delo Gear Lubricants ESI are premium grade, multipurpose gear lubricants.They are formulated with ISOSYN® base stocks and compounded with a unique extreme pressure additive utilizin..
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
See Note 3.
ChevronTexaco Thread Compound
Texaco Thread Compound delivers value through:Ability to meet API requirements for high-pressure thread compounds.Galling prevention — Prevents galling in threaded connections. Joints are easier to..
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
ASTM D445
ExxonMobil Mobil Delvac 50 Synthetic Transmission Fluid
Mobil Delvac Synthetic Transmission Fluid 50 is a fully synthetic, manual transmission lubricant engineered to meet the most demanding extended drain and OEM warranty requirements. It is recommended..
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
ConocoPhillips HD Fleet™ 40 Engine Oil
Description: Conoco HD Fleet Engine Oil is a high-quality, single-grade oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. This oil is highly recommende..
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil
ConocoPhillips Tacna® 2000 NLGI No. 1
Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o..
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil; ASTM D445
Nye Lubricants 5300 (SVLG) Synthetic Oil
Information provided by Nye Lubricants.