Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | |
ExxonMobil Diol 13 RD 40 DIOL railroad oils are a full line of heavy-duty crankcase lubricants for locomotive diesel engines. These products are designed to meet the severe service demands imposed by newer railroad diesel l.. |
|||
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | ASTM D445 |
ExxonMobil SAE 40 Mobilgard M50 Mobilgard M50 by ExxonMobil is a premium, extra high performance 50 TBN engine oil designed for use in the most severe residual-fuelled medium-speed diesel applications found in marine and stationar.. |
|||
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | ASTM D445 |
ExxonMobil 412 Mobilgard 12 Series Mobilgard 12 Series by ExxonMobil are high performance diesel engine oils developed for use in trunk piston engines operating on low sulphur distillate fuels in marine and industrial applications. T.. |
|||
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | ASTM D445 |
ChevronTexaco Gear Compounds EP, ISO 150 FeaturesChevron Gear Compounds EP are multipurpose gear lubricants.They provide good thermal stability, extreme pressure
protection, antiwear and demulsibility, oxidation, rust, corrosion control an.. |
|||
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | |
ChevronTexaco Meropa® 150 Texaco Meropa oils deliver value through:Gear set efficiencies — High thermal stability EP system maintains clean gear and bearing surfaces, minimizing deposits which interfere with effective lubri.. |
|||
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | |
ChevronTexaco Pinnacle® EP 150 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |
|||
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | ASTM D445 |
ChevronTexaco TEGRA® ISO 150 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.The most advanced formulation has been selected to provide superior load carrying and antiwear prop.. |
|||
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | ASTM D445 |
ExxonMobil 412 Mobilgard 12 Series Mobilgard 12 Series by ExxonMobil are high performance diesel engine oils developed for use in trunk piston engines operating on low sulphur distillate fuels in marine and industrial applications. T.. |
|||
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | ASTM D445 |
ExxonMobil SAE 40 Mobilgard M50 Mobilgard M50 by ExxonMobil is a premium, extra high performance 50 TBN engine oil designed for use in the most severe residual-fuelled medium-speed diesel applications found in marine and stationar.. |
|||
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | |
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 40 Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi.. |
|||
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | |
ExxonMobil Diol 13 RD 40 DIOL railroad oils are a full line of heavy-duty crankcase lubricants for locomotive diesel engines. These products are designed to meet the severe service demands imposed by newer railroad diesel l.. |
|||
Kinematic Viscosity at 40°C (104°F) | 142 cSt | 142 cSt | |
ConocoPhillips Conoco® El Mar® Ashless Supreme Oil, SAE Viscosity Grade 40 Conoco® El Mar Ashless Supreme is a premium quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and turbocharged 2-stroke cycle natural gas engines. Engine.. |