Kinematic Viscosity at 40°C (104°F) 167 cSt
167 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8170 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 167 cSt
167 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8170R (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 167 cSt
167 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8170U (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 167 cSt
167 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8172 (829) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 167 cSt
167 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8172R (829RP) (UF) Synthetic Oil
Information provided by Nye Lubricants.