Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 224 cSt | 224 cSt | Base Oil; ASTM D445 |
Nye Lubricants 368A (NC-GP) (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 224 cSt | 224 cSt | Base Oil; ASTM D445 |
Nye Lubricants 368AS (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 224 cSt | 224 cSt | Base Oil; ASTM D445 |
Nye Lubricants NC-GP Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 224 cSt | 224 cSt | ASTM D445 |
ChevronTexaco Delo® 100 Motor Oil, SAE 50 Features:Chevron Delo 100 Motor Oils are high performance crankcase oils for diesel engines.They are manufactured using selected premium paraffinic base oils and detergent, dispersant, wear control,.. |
|||
Kinematic Viscosity at 40°C (104°F) | 224 cSt | 224 cSt | |
ChevronTexaco URSA® SAE 50 Extra Duty Texaco Ursa Extra Duty oils deliver value through:Excellent high temperature deposit control. Protects against high temperature oxidation and oil thickening.Special extreme pressure antiwear propert.. |