Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 29.5 cSt
29.5 cSt
ASTM D445
ExxonMobil Mobil Rarus 824
The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet..
Kinematic Viscosity at 40°C (104°F) 29.5 cSt
29.5 cSt
ASTM D445
ExxonMobil Mobil Rarus 824
The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet..
Kinematic Viscosity at 40°C (104°F) 29.5 cSt
29.5 cSt
ChevronTexaco Capella® WF 32
Texaco Capella WF oils delivers value through:Wax-free — Suitable for ultra-low temperature service.Water-free — Low moisture content prevents icing in refrigeration expansion valves and helps pre..
Kinematic Viscosity at 40°C (104°F) 29.5 cSt
29.5 cSt
ASTM D445
ChevronTexaco ISO 32 Refrigeration Oil WF
FeaturesChevron Refrigeration Oils WF are manufactured using medium viscosity index straight mineral oils. The base stocks are carefully selected to assure the low pour points that are necessary for..