Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 318 cSt | 318 cSt | |
ConocoPhillips Hydroclear® 320 Multipurpose R&O Oil, AGMA Lubricant No. 6 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |