Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 34.4 cSt | 34.4 cSt | |
ChevronTexaco TDH® W Oil Texaco TDH oils deliver value through:Lower operating costs — By delivering or exceeding the performance of fluids supplied by equipment manufacturers, helps in avoiding the cost of generally more .. |
|||
Kinematic Viscosity at 40°C (104°F) | 34.4 cSt | 34.4 cSt | ASTM D445 |
ChevronTexaco THF W FeaturesChevron THF W is a high quality, multifunctional fluid, specially formulated for low temperature use in transmissions, final drives, wet brakes, and hydraulic systems of tractors and other e.. |