Polymer Property : Kinematic Viscosity at 40°C (104°F) = 3400 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 3400 cSt
3400 cSt
ConocoPhillips SynXPA® HC-150 H Lubricant HC-150
Description: Conoco SynXPA H Lubricant is a premium-quality synthetic-polyolester lubricant that offers protection for heavily loaded and partially opened open gears, such as those in ball mills, sh..