Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 44 cSt | 44 cSt | Base Oil; ASTM D445 |
Nye Lubricants 728A (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 44 cSt | 44 cSt | Base Oil; ASTM D445 |
Nye Lubricants 728J (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 44 cSt | 44 cSt | ASTM D445 |
ExxonMobil Mobil Rarus 1025 SHC 1000 Series The Mobil Rarus SHC 1000 Series is a line of supreme performance oils primarily intended for the lubrication of severe duty rotary screw and vane air compressors. They are particularly suited for se.. |
|||
Kinematic Viscosity at 40°C (104°F) | 44 cSt | 44 cSt | |
ConocoPhillips Syncon® 46 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |
|||
Kinematic Viscosity at 40°C (104°F) | 44 cSt | 44 cSt | |
ELM® EnviroLift™ Biobased Elevator Hydraulic Oil Description: EnviroLift™ Biobased Elevator Hydraulic Oil is an advanced, biobased hydraulic oil formulated with the best optimized USA grown natural seed oils that surpass the lubricity of most con.. |
|||
Kinematic Viscosity at 40°C (104°F) | 44 cSt | 44 cSt | ASTM D445 |
ELM® NSF H1 Food Grade Chain and Cable Lubricant Description: ELM Chain Lubricant – Food Grade is a high performance food grade chain lubricant formulated with the best optimized USA-grown natural seed oils and select additives, it surpasses t.. |
|||
Kinematic Viscosity at 40°C (104°F) | 44 cSt | 44 cSt | |
ELM® SoyFluid™ Hydraulic Industrial (ISO 46) Premium Biodegradable – Biobased Hydraulic Oil Description: ELM Biotechbased SoyFluid™ Hydraulic Industrial (ISO 46 & 68) are biodegradable hydraulic oils formulated with the best optimized USA grown natural seed oils that surpass the lubricity.. |
|||
Kinematic Viscosity at 40°C (104°F) | 44 cSt | 44 cSt | ASTM D445 |
ChevronTexaco FM Trolley Oil Chevron Trolley Oil FM is a tasteless, odorless, high viscosity index paraffinic lubricating oil combined with additives that provide lubricity and rust protection, antiwear performance, and tackine.. |
|||
Kinematic Viscosity at 40°C (104°F) | 44 cSt | 44 cSt | ASTM D445 |
ExxonMobil Mobil Rarus 1025 SHC 1000 Series The Mobil Rarus SHC 1000 Series is a line of supreme performance oils primarily intended for the lubrication of severe duty rotary screw and vane air compressors. They are particularly suited for se.. |