Kinematic Viscosity at 40°C (104°F) 467 cSt
467 cSt
ASTM D445
ChevronTexaco Sil-X® NLGI 1 Grease
FeaturesChevron Sil-X Grease is a silica thickened grease. It is manufactured using high viscosity, high viscosity index base oils and contain effective rust and oxidation inhibitors.It is transpare..
Kinematic Viscosity at 40°C (104°F) 467 cSt
467 cSt
ASTM D445
ChevronTexaco Sil-X® SF Grease
FeaturesChevron Sil-X Grease is a silica thickened grease. It is manufactured using high viscosity, high viscosity index base oils and contain effective rust and oxidation inhibitors.It is transpare..