Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 79.1 cSt | 79.1 cSt | ASTM D445 |
ChevronTexaco RPM® SAE 10W-30 Heavy Duty Motor Oil Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha.. |
|||
Kinematic Viscosity at 40°C (104°F) | 79.1 cSt | 79.1 cSt | |
ChevronTexaco URSA® SAE 10W-30 Super Plus Texaco Ursa Super Plus SAE 10W-30 delivers value through:One oil for all services, both diesel and gasoline, minimizes the chance of misapplication.Reduced inventory investment — No need to maintai.. |