Polymer Property : Kinematic Viscosity at 40°C (104°F) = 95.1 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 95.1 cSt
95.1 cSt
ASTM D445
ExxonMobil Heavy Mobil DTE Oil Named Series
The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se..
Kinematic Viscosity at 40°C (104°F) 95.1 cSt
95.1 cSt
ASTM D445
ExxonMobil Heavy Mobil DTE Oil Named Series
The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se..