Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 13.9 cSt | 13.9 cSt | ASTM D445 |
ExxonMobil 627 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.9 cSt | 13.9 cSt | Base Oil; ASTM D-445 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 0 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.9 cSt | 13.9 cSt | Base Oil; ASTM D-445 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 1 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.9 cSt | 13.9 cSt | ASTM D445 |
ExxonMobil 627 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.9 cSt | 13.9 cSt | Base Oil; ASTM D-445 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 2 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |
|||
Kinematic Viscosity at 100°C (212°F) | 13.9 cSt | 13.9 cSt | ASTM D445 |
ChevronTexaco ISO 150 Industrial Oil EP FeaturesChevron Industrial Oils EP are multipurpose oils for industrial service.Chevron Industrial Oils EP are designed to help minimize wear in all types of plant lubrication and also provide long .. |